" In the same year, two other 10-in. columbiads were cast, of the same iron, the one solid, and the other hollow. Both moulds were placed in the same pit, and all the space in the pit outside of the moulds was filled with moulding-sand, and rammed. This... "
Treatise on Iron Ship Building: Its History and Progress as Comprised in a ... - Strana 141
autor/autoři: William Fairbarn (bart., Sir) - 1865 - 313 str.
Úplné zobrazení - Podrobnosti o knize

A Treatise on Ordnance and Armor: Embracing Descriptions, Discussions, and ...

Alexander Lyman Holley - 1865 - 972 str.
...in the same pit, and all the space in the pit, outside of the moulds, was filled with moulding-sand and rammed. " This was done because the iron cases...them to yield and let the iron run out of the mould." The external cooling of the 10-inch hollow gun, by the contact of the flask with green sand, was therefore...
Úplné zobrazení - Podrobnosti o knize

A Treatise on Ordnance and Armor: Embracing Descriptions, Discussions, and ...

Alexander Lyman Holley - 1865 - 1516 str.
...with moulding-sand and rammed. " This was done because the iron cases of the moulds w<-r<- not largo enough to admit the usual thickness of clay in the...mould. It was apprehended that the heat of the great masa of iron within, would penetrate through the thin mould, and heat the iron cases so much as to...
Úplné zobrazení - Podrobnosti o knize

Spons' dictionary of engineering, ed. by O. Byrne (and Spon). 8 div, Svazek 80

Spon E. & F.N., ltd - 1869 - 434 str.
...in the same pit, and all the space in the pit outside of the moulds was filled with moulding-sand, and rammed. This was done because the iron cases of...them to yield and let the iron run out of the mould. The external cooling of the 10-in. hollow gun, by the contact of the flask with green sand, was therefore...
Úplné zobrazení - Podrobnosti o knize

Spon's Dictionary of Engineering, Civil, Mechanical, Military and Naval ...

Edward Spon - 1869 - 406 str.
...in the same pit, and all the space in the pit outside of the moulds was filled with moulding-sand, and rammed. This was done because the iron cases of...mould, and heat the iron cases so much as to cause them tc yield and let the iron run out of the mould. The external cooling of the 10-iu. hollow gun, by the...
Úplné zobrazení - Podrobnosti o knize

Spons' Dictionary of Engineering, Civil, Mechanical, Military, and ..., Svazek 1

Edward Spon, Oliver Byrne, Ernest Spon, Francis N. Spon - 1874 - 396 str.
...in the same pit, and all the space in the pit outside of the moulds was filled with moulding-sand, and rammed. This was done because the iron cases of...penetrate through the thin mould, and heat the iron cases to much as to cause them tc yield and let the iron run out of the mould. The external cooling of the...
Úplné zobrazení - Podrobnosti o knize

Transactions of the American Institute of Mining, Metallurgical ..., Svazek 71

American Institute of Mining, Metallurgical, and Petroleum Engineers, American Institute of Mining Engineers - 1925 - 1476 str.
...flasks were not large enough to admit the usual amount of sand in the walls of the mold. It was feared that the heat of the great mass of iron within would penetrate the thin mold and let the iron run out; consequently the exterior of the mold of the 10-in. hollow...